High Strain Rate Characterization of Mg Alloys

 

Instructions for Use

Step 2: Select Data from Tests to Analyze

Each test contain data from multiple sensors. The definition of test labels can be found by clicking on the link Description of X, Y Labels. Data sets from different tests is selected in X and Y columns of the test table. Only one X item in each test can be selected. Multiple Y items for each test may be selected using standard options in your browser.

The X data has to be of the same type, i.e. selected X labels for all tests to be analyzed have to start with same string, TIME or STRAIN. The Y data also have to be of the same type, i.e. selected Y labels for all tests to be displayed have to start with STRAIN or STRESS.

Test data is included into the graph by checking Plot check-box for the test. Multiple tests may be selected. Generate the graph in a new window by clicking graph button.

Select

Strain derived from LVDT and TIME include the displacement of the overall load train, so that the material will appear more flexible than it is. This excess deformation can be determined and eventually subtracted by examining material deformation in the low strain region (yield region) using direct strain measurement methods. To do so, select X data set as STRAIN FOIL GAGE (electrical resistance strain gage bonded to the gage section of the specimen), or STRAIN VIC GAGE (strain measured by the digital image correlation in the specimen's gage section). The electrical resistance strain gages often debond at larger strains, especially for higher strain rates. In those cases, the data from STRAIN LVDT and/or STRAIN TIME can be appended to the low strain region data, although we need to account for the additional deformation that comes from the entire load train. A simple approach is to:

  1. select a Y value common to the X data sets for STRAIN (FOIL or VIC) GAGE (low strain region) and STRAIN (LVDT or TIME) (high strain region), and
  2. use the low strain region X point for the common Y value as the starting value for the large strain region data from STRAIN (LVDT or TIME).

Measurements from different sensors have different validity regions:

  • Stress derived from LOADCELL data is the most reliable source for the stress data in the lowest strain rate range [0.01, 0.1] /sec.
  • Load WASHER data is the most reliable source for stress data in the strain rate region [1, 10] /sec.
  • Due to signal delay and inertia effect in the above two sensors, the stress measurements in the strain rate regime [50,1000] /sec are based on contact and optical measurement of strains at different locations of the specimen. The stress in the specimen is calculated based on simple elastic relation between stress and strain in elastically deformed tab region. Load WASHER data provides guide for the expected values, but its signals exhibits large oscillations.